在合金铝板的整个生产过程中,不可避免地会遇到许多产品质量问题。一些产品质量问题是由于在整个生产过程中工作人员的粗心大意而引起的,而一些产品质量问题是由于在应用的中后期阶段实际操作不当而引起的。因此,铝板生产厂家实际上可以避免铝板产品质量问题的根本原因。
In the whole production process of alloy aluminum plate, many product quality problems are inevitable. Some product quality problems are caused by the carelessness of the staff in the whole production process, while some product quality problems are caused by improper operation in the middle and later stages of application. Therefore, aluminum plate manufacturers can actually avoid the root cause of aluminum plate product quality problems.
在铝板的生产中,可以避免实际操作和机械设备的使用。铝板存在许多常见的产品质量问题,油渍问题是常见的质量损失之一。油渍并不意味着铝板在生产后会被污染。只是铝板冷轧之后,铝板制造商在铝头的表面上放了太多的油,并且除了轧制的油膜外还添加了剩余的油脂。在产品咨询和批量生产的中后期,您会发现这种脂肪在外面肉眼可见。
In the production of aluminum plate, the actual operation and the use of mechanical equipment can be avoided. There are many common product quality problems in aluminum plate, and oil stain is one of the common quality losses. Oil stains do not mean that the aluminum plate will be contaminated after production. But after the cold rolling of aluminum plate, the aluminum plate manufacturer put too much oil on the surface of the aluminum head, and in addition to the rolling oil film, it also added the remaining grease. In the middle and later stage of product consultation and mass production, you will find that the fat is visible to the naked eye.

铝板生产厂家
许多油脂主要散布在挤出机入口和出口的顶部和底部或辊的颈部。飞溅后,它会滴在盒子的表面上,然后由于挤出机测厚仪的漏油而在挤出机滚筒清洁器中被发现是异常情况,并且这种油的成分很杂而且很脏。由铝板制造商生产的铝板表面上的这种油渍会严重损害合金铝板的外观。
Many oils are mainly distributed at the top and bottom of the extruder inlet and outlet or at the neck of the roller. After splashing, it will drop on the surface of the box, and then due to the oil leakage of the thickness gauge of the extruder, it is found to be abnormal in the roller cleaner of the extruder, and the composition of the oil is very miscellaneous and dirty. This kind of oil stain on the surface of aluminum plate produced by aluminum plate manufacturer will seriously damage the appearance of alloy aluminum plate.
同时,当每个人都评估铝板的质量时,油性缺 陷的数量是关键标准之一。一方面,由于铝板的厚度较薄,在随后的淬火过程中很容易产生泡沫,并且由于表面上残留的油太多,因此在铝的表面会产生大量的残留物。铝板,这也将导致中后期的应用性能不是很好。另一方面,如果铝板的外观足够干净,则可以用作室内装饰和包装产品的美学要求,否则不能售卖。
At the same time, when everyone evaluates the quality of aluminum plate, the number of oil defects is one of the key criteria. On the one hand, as the thickness of the aluminum plate is relatively thin, it is easy to produce foam during the subsequent quenching process, and because there is too much oil on the surface, a large amount of residue will be produced on the surface of aluminum. Aluminum plate, which will also lead to the late application performance is not very good. On the other hand, if the appearance of aluminum plate is clean enough, it can be used as the aesthetic requirements of interior decoration and packaging products, otherwise it can not be sold.
应该立即将其清理干净,并出于某种原因进行适当处理。同时,我们还应清理所生产产品的表面。如果铝板制造商刚开始时有不干净的油渍,则将立即报销产品。如果将油性产品放到仓库或销售市场中,则事后控制产品质量总是比较困难,并且存在许多无法解决的售后服务问题。铝板也很容易刮擦。
It should be cleaned up immediately and properly disposed of for some reason. At the same time, we should clean the surface of the products. If the aluminum plate manufacturer has unclean oil stains at the beginning, the product will be reimbursed immediately. If the oil products are put into the warehouse or sales market, it is always difficult to control the product quality afterwards, and there are many unsolvable after-sales service problems. Aluminum is also easy to scratch.
实际上,有很多原因会导致铝板刮擦,刮擦或敲打。这可能是由于辊子和导辊表面的划痕引起的。铝板上的划痕通常是凹槽状的疤 痕,当它出现在外部时有时会消失或持续。